Jeremy Taylor wrote:
> My last post must been sent just prior to yours.
>
> I actually ended up completely closing up some holes with the acid copper.
Does that mean the alkaline plate was more capable of completely
covering the holes walls with copper than compared to acid copper
plating ? Which bath was better ?
> It' definitely a more aggressive plate.
yes, the acid copper is fast, almost 100% coulombetric
efficient, good throwing power and easy to maintain and setup.
This is why I suspect you have chosen alkaline plating because it
performed better when plating on the ink surface.
Regards,
Adam