Archive of the former Yahoo!Groups mailing list: Homebrew PCBs

previous by date index next by date
previous in topic topic list next in topic

Subject: Re: [Homebrew_PCBs] Re: plated tin as the etch resist

From: "Jeremy Taylor" <jt@...>
Date: 2004-04-02

Thanks for the tip - I'll mix some up tomorrow morning, and err... figure
out a place to put the new pre dip .

JT

http://www.soundclick.com/jtsound

<snip>
> If you dip the tin-lead plated panels in straight peroxide (30% or
> stronger) for 15 or 20 seconds
> Tom