Archive of the former Yahoo!Groups mailing list: Homebrew PCBs

previous by date index next by date
previous in topic topic list next in topic

Subject: Re: [Homebrew_PCBs] Re: Toner Transfer Wow What a Difference! (? Alan King)

From: Alan King <alan@...>
Date: 2003-12-11

Moore wrote:
>>You do not need the coating to desolve to get results. Send the page
>>back through the printer an extra time or two, printing nothing.
>>Extra fusing gets better toner/coating bond.
>
>
> Which side of the paper? i.e. run same as the way originally printed?
>

Won't matter, just print nothing to get the extra heat bonding. It
also seems to make the coating less sticky so the unprinted coating
sticks less and you get a better peel.

Alan