On Thu, May 15, 2014 at 4:24 AM, James
bitsyboffin@... wrote:
> That's the theory. The practice is it's a complete PITA to work with the liquid stuff, very messy, hard to get a good smooth surface without bubbles, exposure time varies radically with colour, thickness of application etc.
>
> For very small boards it's not too bad, but anything over 2 or 3cm per side, it's just frustration city for me.
Thanks for the heads up. At the moment I have neither laminator nor UV source, so all of this is a bit away for me regardless.