On Wed, May 14, 2014 at 10:50 PM, DJ Delorie dj@... wrote:

> My favorite "pretty" trick is to use another layer of etch-resist film
> as a solder mask, over the tin. It gives a deep blue hue to everything.
> http://www.delorie.com/electronics/adapters/r8c-pillar.html

Is there a reason you use etch-resist film instead of an solder mask
proper? I had been considering getting set up for solder mask as well
as Liquid Tin for long-term protection of my boards. I probably will
go that route (solder mask) eventually but for the short term I think
just coating with solder will do just fine.

-p.