Subject: Re: No plating through-hole plating

From: psykhon@...
Date: 2014-02-11

Sorry, I meant to reply to Paul mainly and also to the general discussion

--- In Homebrew_PCBs@yahoogroups.com, "cheater00 ." <cheater00@...> wrote:
>
> On Tue, Feb 11, 2014 at 3:44 PM, <psykhon@...> wrote:
> >
> > Silver and Cooper powder or flask with solder mask a the adhesive/aglutinant
> > Both sides should be laminated with something "peelable" prior to drilling
> > Lots of testing to find the right proportions,but I guess more than 90% metals
>
> Pardon me?
>