| previous by date | index | next by date |
| previous in topic | topic list | next in topic |
>Pardon me?
> Silver and Cooper powder or flask with solder mask a the adhesive/aglutinant
> Both sides should be laminated with something "peelable" prior to drilling
> Lots of testing to find the right proportions,but I guess more than 90% metals