Subject: Re: [Homebrew_PCBs] Stubborn ferric chloride etching.

From: "Geoff Wood" <geoff@...>
Date: 2014-01-10


 
----- Original Message -----
From: richanny@...
To: Homebrew_PCBs@yahoogroups.com
Sent: Friday, January 10, 2014 9:44 AM
Subject: [Homebrew_PCBs] Stubborn ferric chloride etching.

 

Using plain hydrated ferric chloride etch, warmed up a little, the last two boards done have been really stubborn to etch away the bridges between narrow tracks and pads. They needed extended time , so much that some narrow tracks just disappeared under the resist, and the boards scrapped.

Any suggestions?
∗∗∗∗∗∗∗∗∗∗∗∗∗∗∗∗∗∗∗∗∗∗∗∗∗∗∗∗∗∗∗∗∗∗∗∗∗∗∗∗∗∗∗
 
 
Try a fish-tank air-pump to aggitate the solution.
 
geoff
.