Russell,
Thanks for the help.
Rick
___________________________________________
By aerating the ferric chloride (possibly just with bubble etching like i
do), it becomes copper chloride etchant and lasts years. Start off with 1:1
dilution with water. Add a bit (like 5%) HCl acid every few months. Keep
covered when not in use. Disposal is nothing more than flushing money away.