>HCl/H2O2 is very fast anyway, but it could probably be useful for CuCl2.
>
>Leon
-=-=-=-
I found it not so fast. I etched a 5" x 10" 1-sided board (consisting
of several duplicate small circuits) and it took almost an hour. I
started with a fresh batch, just enough etchant to cover the board
but added more as time dragged on.
Maybe my mix is wrong? I'm using 15 percent hcl (muriatic acid) and 3
percent h2o2 at a mix of 1:1.
What mix are you using?
Thanks,
Dave