Archive of the former Yahoo!Groups mailing list: Homebrew PCBs

previous by date index next by date
previous in topic topic list next in topic

Subject: Re: Now

From: "fredbutz" <fredbutz@...>
Date: 2010-07-25

Also, there is a product called Cool-Amp Silver Plating Powder.
http://www.cool-amp.com/cool_amp.html

I've used it some. I plan to do a comparison soon and will let you know

--- In Homebrew_PCBs@yahoogroups.com, Alessio Sangalli <alesan@...> wrote:
>
> Hi, as I am perfectioning my PCB making, I reached a point where I can
> do very good boards, but especially if I am making a bigger, double-face
> one, with huge ground planes, tinning takes simply too much time, and if
> I want to do it properly, I end up wasting a lot of solder wick braid to
> remove the excess tin.
>
> I've read past messages but I was not able to find a method that is well
> documented and can be considered a viable solution for a hobbyst that
> makes only few boards per month.
>
> bye
> as
>