Archive of the former Yahoo!Groups mailing list: Homebrew PCBs

previous by date index next by date
previous in topic topic list next in topic

Subject: Re: developing immersion tank

From: "bhleavi" <bhleavi@...>
Date: 2009-09-16

I use the M G Chemicals Positive Resist boards. When I develop them just after I drop the board in you can see the resist coming off. I would not describe it as Gunk more like a Blue ink. Then just lightly brush over the board several times with a foam brush then rinse good with water I have never used the Neg. resist before.