Subject: Re: [Homebrew_PCBs] What is the best etching solution;

From: "Derward Myrick" <wdmyrick@...>
Date: 2009-04-25

Alessio, I agree with you on this. I do not understand
the people that say the other methods are better.


Derward


----- Original Message -----
From: Alessio Sangalli
To: Homebrew_PCBs@yahoogroups.com
Sent: Friday, April 24, 2009 3:45 PM
Subject: Re: [Homebrew_PCBs] What is the best etching solution;





rickwendel763242 wrote:
> Muriatic Acid (28%) and Hydrogen Peroxid (3%)? Homemade stuff.

This wins HANDS DOWN

It takes 4 minutes in my setup (without any kind of heating)

It is transparent enough in my opinion to see what is happening.

bye
Alessio





[Non-text portions of this message have been removed]