Subject: Re: [Homebrew_PCBs] Shelf life of HCl/H2O2

From: Wayne Topa <linuxone@...>
Date: 2009-01-05

Stefan Trethan wrote:
> Now there's your problem. You don't have CuCl, you have HCl and H2O2.
> The one will keep, the other won't.
>
> You can make CuCl from HCL and H2O2 simply by etching copper, but
> until you get there you have to add H2O2 each time you want to etch.
>
>
Ah Ha, the rejuvination process, adding H2O2 before each etching
session, until it becomes
CuCl. Is that the stage where the solution changes color?

Thanks guys for refreshing my ageing memory.