Archive of the former Yahoo!Groups mailing list: Homebrew PCBs
Subject: Re: [Homebrew_PCBs] Dry film- negative resist... First attempt failure
From: "leon Heller" <leon355@...>
Date: 2008-10-20
----- Original Message -----
From: "Harvey White" <madyn@...>
To: <Homebrew_PCBs@yahoogroups.com>
Sent: Monday, October 20, 2008 8:05 PM
Subject: Re: [Homebrew_PCBs] Dry film- negative resist... First attempt
failure
> On Mon, 20 Oct 2008 15:19:41 -0000, you wrote:
>
>>Hi guys,
>>
>>I tried my first photo process board this weekend and the process
>>failed completely. I am using the dry film, negative resist from MG
>>chemicals.
>
> Negative resist? I'm familiar with the positive resist on precoated
> boards.
>>
>>The failure was in the developing of the resist. While developing,
>>all the resist washed off. It was developed as I could see the
>>traces in the resist, but faintly.
>>
>>The developer solution was a best guess on dilution so this is
>>probably my main failure point.
>>
>
> probably not. For the positive resist it's about 10:1 water to
> developer.
I use 12g NaOH to 1l of water.
Leon
--