> On Sat, 28 Jun 2008, Russell Shaw wrote:
>> Well Geez, i've been etching with the same tank of FeCl for 2 years.
>
> I've been using the same batch of FeCl for over a year (and many boards)
> too, it does seem to last well.
>
> Someone told me that salt helps rejuvinate FeCl - not being a chemistry
> geek I have no idea if this is right or not - is this true or is it BS?
I doubt it. HCl and H2O2 works - I think that the H2O2 oxidises the ferrous
chloride and cuprous chloride to ferric and cupric chloride, and the HCl
provides additional Cl ions.
Leon