Subject: Re: [Homebrew_PCBs] Tin - Plating
From:
DJ Delorie <dj@...>
Date:
2008-06-04
JanRwl@...
writes:
> Doesn't that solution have to be warm (say 140°- 280° F or more) to work
> well?
I've never heated it, seems to work OK. No mention of heating on the
bottle either.