Subject: Re: [Homebrew_PCBs] H2O2 + muriatic acid etchant?
>
> I'm working on switching from FeCl to HCl/H2O2. I'm using Adam's site
> for reference:
> http://members.optusnet.com.au/~eseychell/PCB/etching_CuCl/index.html
>
> My reasoning is that CuCl2 can be regenerated, whereas FeCl eventually
> needs to be discarded.
You can regenerate FeCl3 with H2O2 and HCl. The copper content will become
CuCl2, so you end up with both etchants.