I'm working on switching from FeCl to HCl/H2O2. I'm using Adam's site
for reference:
http://members.optusnet.com.au/~eseychell/PCB/etching_CuCl/index.html

My reasoning is that CuCl2 can be regenerated, whereas FeCl eventually
needs to be discarded.