Archive of the former Yahoo!Groups mailing list: Homebrew PCBs

previous by date index next by date
previous in topic topic list next in topic

Subject: Re: SPAM: Re: [Homebrew_PCBs] Metalized holes

From: Stefan Trethan <stefan_trethan@...>
Date: 2003-05-10

hmm the guys from bungard don't like this.
they say it has too high resistance.

http://www.bungard.com/downloads/ANTI_E.PDF
somewhere in there...

regards
st

10.05.2003 18:30:02, Neil <cobra_neil@...> wrote:

>Here's one system/source for chemical thru-hole plating that I've had laying
>around in my bookmarks....
> http://www.thinktink.com/stack/volumes/volvi/condink.htm
>
>(I've never experimented with this though).
>
>Cheers,
>-Neil.
>
>
>
>On Friday 09 May 2003 19:29, JanRwl@... scribbled:
>> Markus!
>>
>> Please let us know what those "right chemicals" are, and how to apply them!
>> (Temperature? catalysts? time in bath? USW!)
>>
>> Then, what current (Strom, Amperes) per 0.1 m^2 to plate-through!
>>
>> But remember! The plating-through is done BEFORE etching!
>>
>> Thanks! Jan Rowland
>
>
>
>Be sure to visit the group home and check for new Bookmarks and files:
>http://groups.yahoo.com/group/Homebrew_PCBs
>
>To unsubscribe from this group, send an email to:
>Homebrew_PCBs-unsubscribe@yahoogroups.com
>
>
>
>Your use of Yahoo! Groups is subject to http://docs.yahoo.com/info/terms/
>
>
>