Volkan, the breaking fluid indeed works!
I'm amazed, and stumped how you worked that one out.
No more puddling at all - looks great. Now i hope the breaking fluid will
not hamper curing or etching - but i don't expect since everything you
suggest seems to work ;-)
Test PCB next. Hopefully this time it finally works.
ST
On Fri, 14 Jul 2006 19:28:55 +0200, Volkan Sahin <
vsahin@...>
wrote:
> Stefan,
> I saw some puddling when the board is not clean enough and to avoid it
> I used wetting agent. I just did a few tests it worked for me.
> I used automobile break fluid as a wetting agent. Coat cleaned pcb with
> very thin film of break fluid and wipe it several times completely with
> paper towel. Set printer to minimum ink amount and then print.
> Volkan