On Tue, 06 Jun 2006 08:51:03 +0200, Andrew <andrewm1973@...> wrote:

>
> HOWEVER - if you only etch one board in a
> blue moon - Amonia Persulphate or FeCl are
> probably better ideas.


I wouldn't even be sure of that.
There's no disadvantage of CuCl that i can see, so why would the others be
better?
As long as you have enough spare space to store your tank and two bottles
of regenerating chemicals it really seems a good etchant. Of course if one
can get the other etchants easier....