Archive of the former Yahoo!Groups mailing list: Homebrew PCBs

previous by date index next by date
previous in topic topic list  

Subject: Re: Regenerating FeCl3

From: "caveteursus <j.walton@...>" <j.walton@...>
Date: 2003-02-14

It's actually the HCl (hydrochloric acid) which combines with the
copper to form CuCl2 + H. This is why it's not a good idea to etch on
a stove -- hydrogen gas.

This explains the reaction (you'll need powerpoint):
http://www.utep.edu/green/chem2.ppt


--- In Homebrew_PCBs@yahoogroups.com, "caveteursus <j.walton@a...>"
<j.walton@a...> wrote:
> here's a link from QSL NET
>
> http://www.qsl.net/iz7ath/web/02_brew/14_howto/02_clor/