Subject: Re: [Homebrew_PCBs] Re: General Home-Brew CuCl chemistry and technique

From: JanRwl@...
Date: 2005-08-21

In a message dated 8/21/2005 12:42:51 P.M. Central Daylight Time,
phil1960us@... writes:

If you can use FeCl, you can use AP.




OK, Phil; I'm open to that! Then, same question to AP. Where do you get
it? How many gm. of AP to a liter of water? Heated to mix? Warmed to use??
Can it be "regenerated", or is it spent, once it "quits the first time"?
Jan R.