Archive of the former Yahoo!Groups mailing list: Homebrew PCBs
Subject: General Home-Brew CuCl chemistry and technique
From: JanRwl@...
Date: 2005-08-20
Can someone here PLEASE outline the procedure and chemistry to use for this
etch-method? I have never seen ANYWHERE a list like,
"1. Boil the bare blank in swamp-water;
2. Incant;
3. Swish the board around in a 30% CuCl solution over 80°C for 15 minutes;
4, Etc. etc."
With FeCl, you can omit steps 2. and 4., and the result is fine, but messy.
Please?
[Non-text portions of this message have been removed]