>I was of the impression from earlier posts in this thread that the
>stuff you were talking about was lead-free
You can get lead-free plumber's solder paste. You can also get it with
non-acidic flux. Just buy the one you want.
>Seems to me to be a whole lot easier to use than the stuff I've seen
>talked about in the context of surface-mount, where it has a limited
>lifespan, requires refrigeration (!)
I've been using the same jar for about two years, just add water if you
inadvertently leave the jar open and it dries out. Also, you'll be