The melt temp seems to be lower. It goes on very easy. However, being able
to wash is the prime advantage.
Of course, this whole thing is so subjective. There are many acceptable
methods obviously. I like getting all the flux washed off though. It sure
leaves a clean board.
Larry H
----- Original Message -----
From: Mountain Man <mtman at cloud9.net>
To: J. Larry Hendry <jlarryh at iquest.net>; synth-diy
<synth-diy at node12b53.a2000.nl>
Sent: Saturday, May 05, 2001 5:43 AM
Subject: Re: [sdiy] Larry's MOTM/diy/AH pages
I'm curious as to how this kind of solder is easier to use (other than the
fact
you can wash it off). I'm not looking for "squeaky clean" boards, but might
switch if there are other advantages.
Thanks,
Elby
"J. Larry Hendry" wrote:
>
> One could do the whole thing with "no clean" type solder. However, I like
> leaving the boards as clean as possible and the organic stuff is so much
> easier to use. I used one type of solder too before MOTM. But, Paul has
> converted me to his way of thinking. I do all my projects this way now.
>