OK I was in the to process of etching my first PCB board today :) which I
layed out with PNP blue. The problem is, I fixed up the design where PNP
din't adhere to with a sharpie pen (permanent ofcourse). However when i
placed to board into the FeCl, the pen markings came of in about 2 secs :(
Now I heated the FeCl quite a bit, could this have caused the failure?
Ohh I'm using the FeCl from Radio Smut, so maybe its that? Any ideas?
Thanks
yoshi
,,,,
>>>---( oo )--->
********************************oOOo (..) oOOo*******************************
* *
* YOSHIKI OHMURA *
* synthetic fruit laboratories *
* po box 8071 *
* evanston, il 60204-8071, usa *
* tel: (847) 328-5397 fax: (847) 328-5398 mobile: (630) 564-1236 *
* e-mail: yoshi at techno.king.net *
* company e-mail: syntheticfruit at techno.king.net *
* www: http://techno.king.net/synthetic-fruit/index.html *
* *
*****************************************************************************